Dental Materials Journal
Online ISSN : 1881-1361
Print ISSN : 0287-4547
ISSN-L : 0287-4547
Original papers
Tensile Bond Strength of One-step Self-etch Adhesives to Er:YAG Laser-irradiated and Non-irradiated Enamel
Atsushi KAMEYAMAJunji KATOKoya AIZAWATsuyoshi SUEMORIYuichi NAKAZAWATsuyoshi OGATAYoshito HIRAI
Author information
JOURNAL FREE ACCESS

2008 Volume 27 Issue 3 Pages 386-391

Details
Abstract

This study determined the bond strengths to Er:YAG laser-irradiated and non-irradiated bovine enamel of three one-step self-etch adhesives (AQ Bond Plus (AQP), G-Bond (GB), and Clearfil Tri-S Bond (TS)) and one two-step self-etch adhesive (Clearfil Megabond (MB)). Eighty SiC paper-ground bovine enamel surfaces were used, of which half were laser-irradiated. The enamel surfaces were bonded to a resin composite with each adhesive, and tensile bond strengths were determined after 24 hours. For non-irradiated enamel groups, MB achieved greater bond strength to enamel than GB and TS (p<0.05), but no significant difference was found between MB and AQP (p>0.05). For laser-irradiated enamel groups, no significant differences were found among the four adhesives (p>0.05). Additionally, for each adhesive, no significant differences were found between laser-irradiated and non-irradiated enamel. It was thus concluded that Er: YAG laser irradiation of enamel did not affect the tensile bond strength of one-step and two-step self-etch adhesives.

Content from these authors
© 2008 The Japanese Society for Dental Materials and Devices
Previous article Next article
feedback
Top