Smear layer deproteinization with NaOCl and HOCl: Do application/wash-out times affect dentin bonding of one-step self-etch adhesives?
Kittisak SANONTakashi HATAYAMAAntonin TICHYOrnnicha THANATVARAKORNTaweesak PRASANSUTTIPORNTakahiro WADAMasaomi IKEDAKeiichi HOSAKAMasatoshi NAKAJIMA
著者情報
ジャーナル フリー

2022 年 41 巻 3 号 p. 353-362

詳細
抄録

This study investigated the influence of application/wash-out times of sodium hypochlorite (NaOCl) and hypochlorous acid (HOCl) on dentin bond strength of one-step self-etch adhesives (1-SEAs). Human coronal dentin discs with a standardized smear layer were pretreated with 6% NaOCl or 100 ppm HOCl for 5 s, 15 s, or 30 s, and washed out with water for 5 s, 15 s or 30 s with or without the application of Clearfil DC Activator (CDA). No pretreatment was used as a control. The discs were bonded with a 1-SEA (Bond Force II or Clearfil Universal Bond Quick) and microtensile bond strength (µTBS) was measured after 24 h. Pretreatment with NaOCl for 15 s and 30 s significantly decreased µTBS (p<0.05), irrespective of wash-out time. The application of CDA recovered µTBS but did not outperform the control group. Conversely, pretreatment with HOCl for 15 s and 30 s followed by 30 s wash-out time significantly increased µTBS of 1-SEAs (p<0.05), regardless of CDA application.

著者関連情報
© 2022 The Japanese Society for Dental Materials and Devices
前の記事 次の記事
feedback
Top