Factors for Active Site Generation and Pore Development in Fuel Cell Catalysts Formed from Glucose/Nitrogen Source/Fe Salts
Jun MARUYAMANobutaka FUKUIMasayuki KAWAGUCHITakahiro HASEGAWAHiroaki KAWANOTomoko FUKUHARASatoshi IWASAKI
著者情報
ジャーナル フリー

2011 年 79 巻 5 号 p. 318-321

詳細
抄録

A carbon-based noble-metal-free fuel cell cathode catalyst was formed by heat treatment of a mixture of glucose, Fe gluconate, and 1,4-diamino-2,3-dicyano-9,10-anthraquinone as a nitrogen source. The factors for the formation of the active site and the pore development were the heat-treatment temperature and the content of the nitrogen source in the starting mixture. The activity for oxygen reduction was dependent on the active site and the pore development, which were optimized to form the catalyst with the improved activity compared to those formed from various glucose/nitrogen source/Fe salts mixtures

著者関連情報
© 2011 The Electrochemical Society of Japan
前の記事 次の記事
feedback
Top