2011 Volume 51 Issue 4 Pages 544-551
This paper proposes a novel process for the pre-treatment of high phosphorus iron ore by pre-reduction, air jet milling and screening methods. The dephosphorization behavior was evaluated as a function of such parameters as the milling gas kinetic energy, Ek and specific energy consumption, Esp. At a fixed milling gas kinetic energy, the dephosphorization treatment behavior was highly dependent on the solids feed rate and the degree of sintering of the pre-reduced phases. The proposed pre-treatment process involves a pre-reduction process by carbonaceous materials at 1200°C, and air jet milling using Ek of 325.24 kJ and Esp of 3.24 kJkg–1h followed by fine screen separation using a 25 μm screen size.