Grain refinement of AZ31 magnesium alloy sheet produced by melt drag process with super heat treatment
Shinichi NishidaMitsugu Motomura
Author information
JOURNAL FREE ACCESS

2010 Volume 60 Issue 12 Pages 625-628

Details
Abstract
Magnesium alloy is the lightest structural material, so the market such as electrical device is increasing. The purpose of this study is to reveal the effect of superheat treatment for crystal grain size in melt drag process. Melt drag process is one of single roll strip casting process, and strip is made by molten metal directly. Superheat treatment temperature of molten metal are 750~1000, and superheat treatment time are 0~30 min. After superheat treatment, strip was casted by melt drag process. Crystal grain size, strip thickness and Vickers hardness were examined. Minimum crystal grain size is about 12 μm.
Content from these authors
© 2010 by The Japan Institute of Light Metals
Next article
feedback
Top