2026 Volume 90 Issue 10 Pages 186-194
The microstructure and magnetic properties of Fe–3.5Si–1.5Al (mass%) steel fabricated by laser-directed energy deposition (L-DED) were investigated. Scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD) analyses revealed that the specimens consisted of coarse columnar grains extending across melt pool boundaries. A pronounced <001> crystallographic texture aligned with the build direction was also observed, indicating epitaxial grain growth.
The direct current magnetic properties, evaluated using a single-sheet tester, showed a strong dependence on the measurement direction relative to the crystallographic texture. The vertical test piece (VTP), in which the measurement direction was parallel to the <001> texture, exhibited the highest magnetic flux density at 800 A/m (B8), the lowest coercivity (HC), and the lowest hysteresis loss. In contrast, the horizontal test pieces, whose measurement direction was perpendicular to the <001> texture, exhibited inferior magnetic properties.
These results indicate that the superior soft magnetic properties of the VTP originate from the alignment of the <001> texture with the measurement direction, corresponding to the easy magnetization axis of ferritic steel. The present study demonstrates that texture control through the L-DED process is essential for improving the electromagnetic properties of Fe–Si–Al steel.