The 24-year clinical performance of porcelain laminate veneer restorations bonded with a two-liquid silane primer and a tri-n-butylborane-initiated adhesive resin
Mitsuo NakamuraHideo Matsumura
Author information
JOURNAL FREE ACCESS

2014 Volume 56 Issue 3 Pages 227-230

Details
Abstract

This report describes the bonding technique and clinical course of porcelain laminate veneer restorations applied to discolored maxillary incisors and canines. The patient was an 18-year-old woman, and tooth reduction was limited to the enamel. Laminate veneer restorations were made with a feldspathic porcelain material (Cosmotech Porcelain). After try-in, enamel surfaces were etched with 65% phosphoric acid gel, and a tri-n-butylborane-initiated resin (Super-Bond C&B) was applied as a bonding agent. The inner surface of the restorations was etched with 5% hydrofluoric acid gel (HF Gel) and treated with a two-liquid silane primer (Porcelain Liner M), after which the Super-Bond resin was applied. Each restoration was seated with a dual-activated composite luting agent (Cosmotech Composite). After 24 years and 8 months, the restorations are functioning satisfactorily. The luting system and bonding technique described in this report are an option for seating laminate veneer restorations made of silica-based tooth-colored ceramics. (J Oral Sci 56, 227-230, 2014)

Content from these authors
© 2014 by Nihon University School of Dentistry
Previous article Next article
feedback
Top