2000 年 12 巻 3 号 p. 365-366
The ceramic foam were prepared by silicon, sodium hydroxide and sodium fluoride. The influence of temperature on volume and weight change was investigated between 423K and 973K. The volume swelling rate of the sample increased with increasing temperature. The value of maximum volume swelling sample was 1382% at 773K for 10 to 20min.