1955 Volume 24 Issue 4 Pages 20-24
In order to investigate the effect of Mo for the low temperature brittleness, the mild steel deposited metals (low hydrogen) containing up to 0.28 % Mo are used. Charpy impact test are carried out in the temperature range of -70°C-100°C.
The transition temperature raises in the range.of 0-0.12% Mo, then lowerizes in the range of 0.12-0.28%o Mo. About thes phenomena and the shape of Energy/Temperature curves some dislocational considerations are persued.