2段繰り返し荷重下における単点スポット溶接継手の疲れ寿命について
軟鋼と高張力鋼の場合の比較
阿部 博司横峯 達也中岡 豊人佐藤 次彦
著者情報
ジャーナル フリー

1993 年 11 巻 2 号 p. 313-320

詳細
抄録

This paper deals with an effect of the load hysteresis on the fatigue life of single spot-welded joint specimen of tensile-shear type for mild steel (SPCC) and high strength steel (HT50) of 0.8 mm in thickness under 2-steps repeating load. Main results obtained are summarized as follows:
(1) The fatigue life for SPCC is generally longer than one for HT50 under usual constant amplitude repeating load, but it is possible that the fatigue life for HT50 is very longer than one for SPCC under the specific repeating load condition.
(2) It becomes clear that fatigue life is considerably influenced according to mechanical properties of spot welds, and fatigue damage due to each load of 2-steps repeating load is not independent each other and can not be discussed without considerations on the hysteresis effect of each load.

著者関連情報
© 一般社団法人 溶接学会
前の記事 次の記事
feedback
Top