J-STAGE トップ  >  資料トップ  > 書誌事項

鉄と鋼
Vol. 88 (2002) No. 6 P 347-354

記事言語:

http://doi.org/10.2355/tetsutohagane1955.88.6_347


The immobilization of fluorine dissolved from hot metal pretreatment slag has been studied by using synthesized compounds such as calcium aluminates, calcium silicates, calcium aluminum silicates and calcium aluminum ferrites. Fluorine ion can be immobilized strongly by 3CaO · Al2O3, and moderately by 3CaO ·SiO2. The F immobilization capability of calcium aluminum silicates decrease with increasing SiO2 content. Fluorine is effectively immobilized by calcium aluminum ferrites due to low hydration rate. The immobilization of fluorine proceeds effectively by using a secondary refining slag with low contents of SiO2 and total Fe.

Copyright © 一般社団法人 日本鉄鋼協会

記事ツール

この記事を共有