In this study, a novel heat/CO2-assisted acid-soluble collagen (HCASC) extraction method was developed to efficiently obtain type I collagen-gelatin blends from Tilapia fish scales. The methodology employed thermal treatment and CO2 infusion in an acidic solution to optimize the yield and sterilization of the extracted compounds. Type I collagen-gelatin blends were extracted using a combination of varying temperatures (40 °C or 90 °C) and acetic acid concentrations (0.1 M or 0.5 M) with the infusion of CO2 microbubbles. This study aimed to address the limitations of the conventional process with respect to yield and to evaluate its characteristics and bioactivity. Through HCASC extraction, the highest yield of type I collagen-gelatin blends was 55.1% at 90 °C in 0.5M acetic acid, as quantified using the Sirius Red assay. Scanning electron microscopy (SEM) images revealed a porous, fibrous structure of the blends, with average fiber diameters ranging from 1.02–3.6 μm. The presence of triple helical structures in the samples was determined using attenuated total reflectance Fourier transform infrared spectrometry (FT-IR/ATR) and circular dichroism (CD) analyses. In vitro cell viability and scratch wound healing assays demonstrated the biocompatibility and wound healing capacity of the blends. Moreover, the samples subjected to heating at 40 °C in 0.1 M or 0.5 M acetic acid, and at 90 °C in 0.5 M acetic acid demonstrated cell viability and wound healing properties. Consequently, type I collagen-gelatin blends have potential applications in skin dressings
Glycol lignin is a type of technical lignin extracted from lignin with polyethylene glycol and is a polyphenolic polymer. In addition to its high heat resistance, polyphenolic polymers have a structure that approximates the graphite structure of carbon fiber, so high adhesion with carbon fiber is expected. In this study, we investigated the effect of adding glycol lignin to the matrix resin to improve the mechanical and thermo-mechanical properties of CFRTP. CFRTP with glycol lignin was prepared by adding glycol lignin to the base resin of an in-situ polymerizable thermoplastic epoxy resin, then adding a catalyst and applying the resin to carbon fiber fabrics, followed by heat press molding to promote polymerization while impregnating the resin into the carbon fiber bundles. The mechanical properties of the fabricated CFRTP were evaluated, and the following findings were obtained regarding the effect of glycol lignin addition. The interfacial shear strength between carbon fiber and the resin increased as the amount of glycol lignin increased. On the other hand, for resins with more than 20 wt% glycol lignin, the fracture strain was lower than the fracture strain of the carbon fiber. As a result, the maximum flexural strength of CFRTP was obtained at a glycol lignin addition of 10 wt% due to the balance between the increase in interfacial shear strength and the decrease in the fracture strain of the resin. This flexural strength was about 9% higher than that of CFRTP without glycol lignin. Furthermore, as the amount of glycol lignin added increased, the CFRTP tended to deform more easily at low temperatures, while maintaining a certain storage modulus in the high temperature range above 140 °C.