ISIJ International
Online ISSN : 1347-5460
Print ISSN : 0915-1559
ISSN-L : 0915-1559
Virtual issue
Current issue
Displaying 1-25 of 25 articles from this issue
Publication Data
Fundamentals of High Temperature Processes
Regular Article
  • Huanhuan Xu, Jintao Gao, Xi Lan, Xiang Ji, Xiang Li, Zhancheng Guo
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1465-1475
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 15, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    Low-grade Bayan Obo niobium concentrates are difficult to utilize because of their complex mineralogy, low niobium grade, and poor selectivity of conventional carbothermic processes. To address these challenges, a novel hydrogen reduction-stepwise smelting separation process based on a hydrogen-carbon coupled metallurgical concept was developed for the staged utilization of Fe–Nb–RE–Ti resources. The proposed process integrates selective hydrogen reduction, carbon-free melting separation, and carbothermic reduction through the intentional retention and inheritance of FeO between process stages. Hydrogen reduction at 800°C produced direct reduced iron (DRI) with a metallization degree of 85.88%. Subsequent carbon-free melting separation at 1500°C yielded metallic iron with a purity of 99.89 wt.% and generated a Nb-enriched primary slag without external flux addition. Carbothermic reduction of the primary slag at 1550°C and a basicity of R=1.0 produced a FeNb alloy containing 11.19 wt.% Nb, while retaining RE and Ti in secondary slag. As a result, three value-added products, namely high-purity iron, FeNb alloy, and RE-enriched slag, were obtained through staged processing. Overall recoveries for Fe, Nb, RE, and Ti reached 96.26%, 87.18%, 96.76%, and 91.18%, respectively. Life-cycle assessment revealed that the process carbon footprint was 17.90 kg CO2/kg alloy when green hydrogen was employed, representing a 53% reduction compared with the conventional route. The proposed process enables efficient stepwise separation and coordinated recovery of Fe, Nb, RE, and Ti from low-grade niobium concentrates, establishing a staged utilization pathway for this type of polymetallic resource and offering a novel green smelting approach for sustainable metallurgy.

  • Ryohei Aoyama, Atuki Ota, Haruto Tateiwa, Takashi Nagai
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1476-1482
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 30, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    When recycling scrap iron, impurities that are difficult to remove, called tramp elements, become a problem. Among them, tin (Sn) has many opportunities for contamination and affects the processability of steel; therefore, new removal methods are needed. Sn is highly reactive with iodine(I) and forms a metal iodide gas at high temperatures. The purpose of this was to remove Sn from iron scrap using I. We prepared carbon-saturated iron containing 2 mass% Sn as a sample, weighed 0.1 g, and placed it into the furnace. Subsequently, I2 gas was injected introduced into the furnace. The Sn concentration and Sn removal rate were calculated by dissolving the sample after the experiment and performing an analysis using ICP-OES. Consequently, the Sn concentration in the sample was reduced to 0.008%, and the removal rate was up to 99.5%.

Ironmaking
Regular Article
  • Kensuke Kumeda, Tamana Ichida, Shuji Ohsaki, Satoru Watano, Shohei Fuj ...
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1483-1491
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 02, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML
    Supplementary material

    In the iron-making process, wet granulation is a key process for utilizing dephosphorized fine ore powders as a raw material. However, dephosphorized ore powders with higher degree of reduction can result in a significant decrease in strength of the green pellets. Moreover, pellet-strength-enhancing effect by adding quicklime was less pronounced in reduced iron ore powder. Therefore, it is essential to investigate the underlying mechanisms that are responsible for the less binder efficiency of quicklime in reduced fine ore powders. To this end, this study investigated effect of quicklime addition on the compressive strength of green pellets prepared from magnetite and hematite. The results exhibited that the addition of quicklime to hematite can significantly enhance their green pellet strength, whereas the addition to magnetite resulted in no strength-enhancing effect on the pellet. The agitation torque of wet powder samples suggested that in the hematite the quicklime reacted well with added water, enhancing the plasticity of the wet powder. In contrast, in the magnetite the quicklime was unlikely to react with water, resulting in much less plasticity-enhancing effect. From several characterizations, wettability of the ore powder was considered to be a key property causing this contrasting response. A mechanistic scenario arising from hydration reaction of quicklime and subsequent formation of fine particles was proposed as a cause of the contrasting response. Finally, it was demonstrated that the green pellet strength can be significantly increased by using ground quicklime.

  • Qing-shi Song, Jie Wu, Alei Domingues, Wei Qi, Cheng-yi Ding, Tie-jun ...
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1492-1502
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 30, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    To investigate the mechanism of steam injection on the sintering process under varying iron ore blending structures, this study conducted sinter pot experiments using two typical ore blends: one with a higher proportion of Australian limonite (Scheme 1) and the other with an increased proportion of Brazilian hematite (Scheme 2). Key injection parameters (duration, start time, flow rate, and pressure) were systematically optimized. The results show that steam injection significantly enhances sintering performance, with the optimal parameters being scheme-dependent. Under optimal conditions, Scheme 2 achieved a 12.1% increase in combustion speed, a 0.3% increase in yield, and a 4.5% increase in productivity compared to Scheme 1. Flue gas analysis revealed a distinct “low O2, high CO2, and high CO” pattern, indicating a shift from conventional solid-gas combustion to a more efficient gas–solid composite combustion mode triggered by the water–gas reaction. Mineralogical analysis further showed that Scheme 2 exhibited lower porosity and improved sinter strength. This study demonstrates that the effectiveness of steam injection is closely tied to the raw material structure, and the optimized synergy between steam parameters and ore blending provides a theoretical basis for precise “one-material-one-strategy” control in industrial sintering processes.

  • Rochim Bakti Cahyono, Asful Hariyadi, Ariany Zulkania, Ade Kurniawan, ...
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1503-1508
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 30, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    The use of biomass as an alternative reduction agent in the iron production process is an important concern in efforts to reduce dependence on fossil fuels and reduce CO2 emissions. This study compares two approaches to biomass utilization, namely biomass pellets–iron ore and carbonized ore obtained through impregnation of biomass/coal tar into porous iron ore. Reductions were carried out on low-grade iron ore from Indonesia, which was characterized through the analysis of XRD, TGA/DSC, and the composition of the reaction gases. The results showed that the carbon in carbonized ore is better distributed in the pore structure, resulting in higher reduction efficiency at temperatures below 1000°C compared to the pellet method. The activation energy of the reduction reaction is also lower in carbonized ore, especially in the formation stage of iron metal (Fe). The addition of biomass of up to 15% to carbonized ore has been shown to be able to complete the reduction reaction completely and eliminate the wustite phase. The gas release characteristics of CO, CO2, and H2 show different stages of devolatilization and reduction between methods, with more controlled gas release in carbonized ore. Overall, the results show that the combination of carbonized ore and biomass additive methods provides superior reduction performance, making it a potential sustainable solution for the iron industry in the future.

  • Nathan A. S. Webster, Dylan Guja, Shu Huang
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1509-1518
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 02, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    The effects of Al2O3 concentration and cooling rate on the crystallisation during cooling of SFCA-III were investigated using in-situ X-ray diffraction. Experiments were conducted at an oxygen partial pressure of 5 × 10−3 atm in the range 298–1623 K and using synthetic iron ore sinter mixtures with basicity (CaO/SiO2 ratio) of ~4. They showed that SFCA-III formed as the first phase to crystallize, from a high temperature phase assemblage comprising magnetite and melt, when the Al2O3 concentration in the mixture was at or above 0.33 mass%. At 0.22 mass% Al2O3, SFCA-III did form however β-CFF was the first phase to crystallize from the melt. At 0.09 mass% Al2O3, the key diagnostic in-situ XRD peak for SFCA-III was almost indistinguishable from the background X-ray intensity and, therefore, the lower limit of Al2O3 concentration where SFCA-III is observed to form during cooling at pO2 = 5 × 10−3 atm is close to 0.09 mass%. Cooling rate experiments showed that for the mixture with 1 mass% Al2O3, SFCA-III was preserved to 298 K when the cooling rate below 1433 K was at or above 17.5 K min−1, after a regime of slower cooling at 2 K min−1 in the range 1623–1433 K. Finally, in separate experiments involving change in pO2 during cooling, we found tentative evidence that SFC-III does form in the Al2O3-free system, albeit within a narrow temperature range and with low abundance. These results further the understanding of the compositional and thermal factors that govern SFCA‑III formation during iron ore sintering.

Steelmaking
Regular Article
  • Tianhao Di, Yize Zhang, Kun Song, Fei Zhao
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1519-1529
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 30, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    During the process of electric arc furnace (EAF) steelmaking, the coherent jet plays a vital role in stirring and decarburization of the molten bath. Its flow field characteristics are influenced by the parameters of the shrouding gas. Improving the impact capability of coherent jets has been a hot research topic in recent years, with one method being the use of supersonic shrouding gas, known as supersonic combustion coherent jet technology. However, the mechanism by which a supersonic shrouding gas influences the main oxygen jet remains unclear. To investigate and quantify the effect of the shrouding gas parameters on the main oxygen jet, the flow fields of the SC coherent jet under different shrouding gas parameter conditions are investigated by both numerical simulation and combustion experiment. The results show that the potential core length of the main oxygen jet is negatively correlated with both the shrouding gas temperature and the distance between the shrouding gas and the main oxygen jet. The effect of the shrouding gas Mach number on the potential core length of the main oxygen jet shows a staged variation. Furthermore, a quantitative relationship between the potential core length of the SC coherent jet and the shrouding gas parameters is established.

  • Hang Ding, Huixiang Yu, Guosen Zhu, Yun Han, Chunyang Liu
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1530-1540
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 07, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    The effect of Al content on the slag/steel reaction between quenching and partitioning (Q&P) steel with refining slag was investigated at 1873 K in a vertical Si–Mo heated furnace. The results shows that the chemical compositions of the steel and slag changed significantly as the Al content in steel increased. After the reaction between slag and steel, the Al content in the steel and the SiO2 in slag increased for the experiment with 0.03% Al content. While in the experiment with high Al content (0.2% ,0.8% and 1.5% Al), Al content in steel and SiO2 content in slag decreased. Thermodynamic analysis revealed that the main reducing agent was Si in the slag/steel reaction for the 0.03% Al steel, whereas it changed to Al for the steel contain 0.2% to 1.5% Al, which resulted in the opposite trend of the slag and steel compositions. In all experiment, the Mg content increased with increasing Al content. The characteristics of inclusions also evolved significantly with increasing initial Al content. In the experiment with Al content of 0.03%, 0.2%, 0.8%, the initial inclusions are mainly MnS. The inclusion changed into MgO and CaO–MgO–Al2O3 after the slag/steel reaction. For the experiment with 1.5% Al, the initial inclusions are mainly AlN and MnS, and it changed into CaO–MgO–Al2O3 after the slag/steel reaction. The variations in Al content exerted a significant influence on the reaction between the Q&P steel and refining slag.

  • Qing Liu, Min Wang, Ziyu Lyu, Hongbin Yu, Yanping Bao
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1541-1556
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 07, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    The magnetic properties of high magnetic induction grain-oriented silicon steel are closely related to the contents of Al and Ti and the characteristics of oxide inclusions. To realize the synergistic control of Al and Ti contents and oxide inclusions in the steel, thermodynamic and kinetic theoretical prediction models were established in this study, and the composition of the CaO–SiO2–Al2O3–MgO slag system was optimized via high-throughput calculations. The effect of MgO content on the low-melting point region of the slag system was analyzed using FactSage 8.3 software, and the optimal MgO content was determined to be 6%–8%. Thermodynamic models for slag-steel equilibrium and mathematical models for inclusion separation and dissolution were established to reveal the regulation mechanisms of basicity and CaO/Al2O3 ratio on the contents of Al and Ti as well as inclusion behavior. Finally, the optimal refining slag composition was determined as follows: CaO=46–52%, SiO2=18–24%, Al2O3=18–24% and MgO=6–8%. Industrial test verification showed that this slag system could stably control the soluble aluminum content in steel at around 0.029%, with aluminum loss less than 0.0030%, residual Ti content less than 0.0020%, and total oxygen content reduced to 0.0006% to 0.0007%. The inclusion number density was within 5 particles/mm2, with an average size of approximately 1.7 µm, mainly composed of SiO2-rich oxides, indicating a significant improvement in molten steel cleanliness. Correspondingly, heats refined by the optimized slag exhibit superior magnetic properties, featuring low core loss of 0.819–0.823 W/kg and high magnetic induction of 1.924–1.925 T.

Casting and Solidification
Regular Article
  • Xingyun Yang, Xinning Zhang, Guanglong Li, Xinming Liu, Wendong Xu, Yi ...
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1557-1566
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 07, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    This study investigates the effects of austempering temperature on the microstructure, mechanical properties, and wear behavior of Cu–Ni-alloyed austempered ductile iron (ADI). Microstructural characterization using optical microscopy (OM) and scanning electron microscopy (SEM) reveals that decreasing the austempering temperature refines the ausferritic matrix, which consists of acicular ferrite and carbon-enriched austenite. The specimen austempered at 260°C exhibited the highest ultimate tensile strength and Brinell hardness, reaching 1440 MPa and 470 HB, respectively, while its elongation was 1.5%. These results reflect the high-strength, high-hardness, and low-ductility characteristics associated with low-temperature austempering. Wear resistance increased with decreasing austempering temperature and reached its maximum at 260°C. This superior wear resistance is attributed to the combined effects of the refined ausferritic microstructure, graphite nodules, and protective oxide layers formed during sliding. Combined analysis of wear loss, friction coefficient, three-dimensional surface topography, two-dimensional depth profiles, and worn-surface morphology confirms the highest wear resistance at 260°C and indicates abrasive wear as the dominant wear mechanism.

Instrumentation, Control and System Engineering
Regular Article
  • Horas Sotardodo Siagian, Yoshihiko Oishi, Sho Osanai, Tambang Manik, K ...
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1567-1579
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 02, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    Wear in slurry systems is strongly influenced by the combined action of erosion and corrosion, making it essential to understand how flow conditions and particle characteristics affect material degradation. This study investigates erosion–corrosion behavior using a rotational Taylor vortex device and develops a predictive model for estimating mass-loss rates. Experiments were conducted on SS400 steel using silica sand particles of fine, medium, and coarse sizes at concentrations of 0, 10, and 30 vol% over a range of Reynolds numbers. Under particle-free conditions, the mass-loss rate increased with Reynolds number due to enhanced corrosion. In contrast, under slurry conditions, the mass-loss response exhibited a non-linear trend, with a decrease observed at higher Reynolds numbers, indicating the presence of a corrosion-resistance effect. Based on the experimental mass-loss-rate trends, a predictive model was developed to estimate mass-loss rates by separating erosion-related and corrosion-related contributions, while implicitly accounting for their interaction through an empirical formulation. The model showed good agreement with experimental data across all test conditions. The proposed framework provides a practical method for evaluating erosion–corrosion behavior and quantifying the relative contributions of erosion and corrosion in vortex-driven slurry environments.

Chemical and Physical Analysis
Regular Article
  • Tomoki Maruoka, Yasuhiro Hoshiyama
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1580-1588
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 13, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    This study aims to develop reference specimens for hydrogen analysis to advance characterization techniques in metallic materials by investigating the fabrication process of sintered alloys composed of titanium and titanium hydride powders. A random forest machine learning algorithm was employed to construct prediction models for density and hydrogen concentration based on sintering conditions. Sintered alloys were fabricated under conditions outside the training dataset to validate the models. Comparisons between the predicted and measured values showed prediction errors within a few percent for both target variables. Furthermore, glow-discharge optical emission spectroscopy showed relatively small positional variations in the hydrogen distribution of the sintered compacts. These results suggest that sintered titanium–titanium hydride alloys have potential for use as reference specimens for quantitative hydrogen analysis and that machine learning holds strong potential for the design and optimization of processes in metallic material systems.

  • Yasuo Takeichi, Yusei Ito, Yasuhiro Niwa, Reiko Murao, Masao Kimura, K ...
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1589-1595
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 08, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML
    Supplementary material

    Gigapixel Fe K-edge imaging XAFS was developed to visualize iron ore sinter over a cm-scale field of view with submicron lateral spatial resolution. By applying singular value decomposition to XANES image stacks, Fe chemical phase maps were obtained for sinter specimens exhibiting distinct microstructures classified as relatively low- and high-temperature sintering textures. The improved spatial resolution enabled direct interpretation of fine sinter textures, including individual hematite grains and acicular calcium ferrite, without the auxiliary optical microscopy required in our previous study. In addition, the polarization dependence of hematite XANES was used to obtain hematite crystal orientation maps. Comparison with EBSD showed that the imaging XAFS orientation contrast was consistent with the crystallographic orientation observed by EBSD. The orientation maps revealed that skeletal hematite forms crystallographically coherent domains across apparent gaps between branches, which is consistent with growth from dendritic hematite. This orientation information further enabled the segmentation of primary and secondary hematite. The results demonstrate that gigapixel imaging XAFS provides simultaneous chemical-state and orientation-sensitive information for microstructural interpretation of iron ore sinter.

Forming Processing and Thermomechanical Treatment
Regular Article
  • Mingfang Wang, Anrui He, Yuxin Zhang, Jianwei Zhao, Chaoyang Li, Chao ...
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1596-1610
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 30, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    The entry temperature of finish rolling is a critical process parameter in hot-strip production, particularly in endless rolling, where the high proportion of thin-gauge products makes rolling stability, energy consumption, and product performance highly sensitive to temperature non-uniformity. The DSCCR (Donghua Strip Continuous Casting and Rolling) process involves multi-stage coupling of heating, rolling, and reheating, while the periodic combustion reversal in regenerative furnaces further complicates temperature control. To address this issue, a temperature-field prediction framework combining a full-process two-dimensional transient heat-transfer model with parameter optimization was developed. A genetic algorithm was employed to calibrate correction coefficients for air cooling, furnace heating, and roll contact by minimizing the mean absolute error (MAE) across three key process stages.

    Results indicate that optimization reduced the model’s MAE and root-mean-square error (RMSE) from 7.506°C to 4.534°C and 8.967°C to 6.504°C, respectively. An independent holdout validation yielded an MAE of 4.486°C and RMSE of 6.570°C (reductions of 38.2% and 26.1% relative to the baseline). The close agreement between the optimization- and validation-set errors demonstrates that the calibrated coefficients maintain stable out-of-sample performance for an independent production batch of the same steel grade under similar operating conditions. Furthermore, the calibrated model quantitatively evaluated the effects of key process parameters and revealed the full-process thermal evolution mechanism. This physics-guided framework provides a reliable theoretical basis for precise temperature control, process optimization, and anomaly diagnosis in the endless rolling of ultra-thin strip steel.

Surface Treatment and Corrosion
Regular Article
  • Misaki Masatsugu, Shintaro Yamanaka
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1611-1618
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 14, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    The growing adoption of electric vehicles (EVs) places increasing demands on lithium-ion batteries (LIBs) to deliver both higher electrochemical performance and reliable safety under abnormal conditions. For prismatic LIBs used in EV applications, aluminum alloys are commonly employed as cell case materials; however, their relatively low melting point raises concerns during thermal runaway. Consequently, Ni-coated steel sheets have been investigated as alternative materials because of their higher melting point and superior mechanical strength. In recent prismatic battery designs, laser welding has been increasingly adopted; however, partial melting of the Ni coating within the weld zone may affect corrosion behavior in the battery electrolyte. In this study, the corrosion behavior of laser-weld zones in Ni-coated steel sheets was examined in LIB electrolytes. Localized electrochemical measurements and long-term immersion tests were conducted in a standard electrolyte and in an electrolyte containing 300 ppm water. The dissolution behavior of Fe ions was evaluated, and the influence of dissolved Fe ions on battery performance was investigated using lithium-ion cells fabricated with Fe-ion-containing electrolytes. Although the weld zones showed slightly higher initial Fe dissolution than the non-welded zones, no clear increase was observed with extended immersion time under the tested conditions. Moreover, no noticeable difference in capacity retention was observed over 40 charge–discharge cycles. These results suggest that, within the experimental conditions of this study, the corrosion behavior of laser-weld zones is comparable to that of non-welded zones.

  • Tomonari Hiraguchi, Junichi Kitagawa, Yoichiro Yamanaka
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1619-1626
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 15, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    In can industry, film-laminated materials are being commercialized as environmentally friendly alternatives to painted ones. Polyethylene terephthalate (PET) film is widely used as a laminating material for steel sheets in beverage and food cans because of its excellent formability, corrosion resistance, and adhesion properties. In food cans, steam retort treatment is used for sterilization. However, the discoloration phenomenon, known as retort blushing, resulting from the exposure of the can’s outer surface to water vapor, has emerged as a significant issue. To mitigate retort blushing, it has been found effective to use a film that blends polybutylene terephthalate (PBT), which crystallizes rapidly, with PET. This method increases the crystalline content in the film during steam retort processing, thereby enhancing its barrier properties against water vapor. Nevertheless, the effect of the crystalline state produced by this method on retort blushing remains unclear. Therefore, we investigated the influence of the PET film’s crystalline state on retort blushing by subjecting the PET film laminated steel sheets to heat treatment, which were manufactured by changing the lamination temperature, and analyzing the crystalline structure using Raman spectroscopy. Our study revealed two key findings: (1) Simply changing the lamination conditions to control the oriented crystalline content does not completely prevent retort blushing, but applying heat treatment after lamination can fully suppress it. (2) Heat treatment induces isotropic crystal growth within the PET film near the interface with the steel sheet, which is believed to prevent the vaporization and expansion of moisture during the retort process, thereby preventing void formation and effectively mitigating retort blushing.

  • Yoshiaki Toda, Nina Kobata, Xianglan Li, Masahiko Demura
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1627-1637
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 15, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    9Cr ferritic/martensitic steel and 18Cr austenitic steel were exposed to steam (0.5 MPa), subcritical water (10.2 MPa), and supercritical water (22.7 MPa) at 650°C for various durations. The pressure dependence of the oxidation rate constants of both steels was determined from the time dependence of specimen weight gain and oxide scale thickness due to oxidation. The oxidation rate constants of both steels decreased with increasing pressure. In steam, the oxidation rate constant of the 18Cr steel was smaller than that of the 9Cr steel. The difference in the oxidation rate constants between the two steels decreased with increasing pressure, and the oxidation rate constants became almost identical in supercritical water. The decrease in the oxidation rate constant with increasing pressure is considered to result from the reduction in voids in the formed oxide scales, which restricts the transport of metal and oxygen ions through the oxide scales.

Transformations and Microstructures
Regular Article
  • Taiki Suzuki, Keita Nakayama, Akinori Yamanaka
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1638-1649
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 05, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML
    Supplementary material

    An accurate prediction of the austenite-to-ferrite (γ → α) phase transformation using the multi-phase-field (MPF) model requires both the incorporation of thermodynamic calculations based on the CALPHAD method and the identification of model parameters. In this study, a Markov chain Monte Carlo (MCMC)-based parameter-estimation framework was developed to evaluate model parameters and their uncertainties using experimental data. To reduce the computational cost of the MPF simulation and enable parameter estimation within a reasonable computational time frame, neural-network surrogate models were constructed to perform thermodynamic calculations. By introducing surrogate models, the MPF simulation was accelerated by more than 220 times compared with conventional MPF simulations coupled with Thermo-Calc software. Subsequently, the developed framework was validated through numerical experiments in which we checked whether the framework can estimate ground-truth parameters using synthetic data obtained from an MPF simulation. The results demonstrated that the framework can accurately estimate the parameters and their uncertainties over a wide range of experimental uncertainties. Furthermore, the developed framework was applied to estimate the interfacial mobility and its uncertainty from the evolution of the α-phase volume fraction during the isothermal γ → α transformation in an Fe–0.19C–1.00Mn (wt.%) alloy. The estimated interfacial mobility parameter was of the same order of magnitude as values reported in previous studies, supporting its physical plausibility. Overall, this study contributes to the accurate prediction of microstructural evolution during the γ → α phase transformation by providing a framework for estimating the model parameters and quantifying their uncertainties based on experimental data.

New Materials and Processes
Regular Article
  • Masahiro Kusano, Kentaro Wada, Makoto Watanabe
    Article type: Regular Article
    2026Volume 66Issue 12 Pages 1650-1668
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 05, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML
    Supplementary material

    In laser powder bed fusion (L-PBF), near-net-shape products are fabricated through the repeated alternation of powder spreading on the build platform and selective melting/solidification by laser scanning. The thermal history during the L-PBF process determines the microstructure and mechanical properties of the built sample. Previous studies have reported that the thermal history is influenced not only by laser scanning parameters, but also by the geometry of the build. In this study, a bipyramidal sample was fabricated from SUS304L powder to understand the relationship between geometry-induced heat accumulation and the resulting microstructures and mechanical properties. The thermal history was investigated by in situ process monitoring and multi-scale thermal analysis. The interlayer temperature at the top surface during the process varied significantly with the bipyramidal geometry, ranging from below 100°C to above 500°C. This interlayer temperature also affected melting and solidification on a microscopic time scale, thereby altering the melt-pool shape, cooling rate, and temperature gradient. Furthermore, the intertrack temperature increased near the pyramid apex because the heat deposited by adjacent laser tracks did not fully diffuse before the next scan pass occurred. Despite these pronounced variations in thermal history, the as-built sample showed only slight site-dependent variations in average grain size, KAM value, non-twin-related HAGB density, and hardness, which generally followed the geometry-dependent trends in thermal history.

Fundamentals of High Temperature Processes
Short Article
  • Hitoshi Muneoka, Yusuke Noda, Takahide Gunji, Tsuyohito Ito, Kazuo Ter ...
    Article type: Short Article
    2026Volume 66Issue 12 Pages 1669-1674
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 30, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML
    Supplementary material

    Anode erosion during molten oxide electrolysis (MOE) remains a fundamental barrier to carbon-neutral ironmaking. In this paper, we demonstrate plasma MOE—in which a direct-current arc plasma serves as the anode to eliminate direct solid-electrode immersion in the melt—under high-temperature ironmaking conditions not previously explored, using an FeO–Al2O3 melt at ~1700 K under an argon atmosphere. Plasma MOE reduced solid-electrode erosion by one to two orders of magnitude relative to that obtained using immersed-electrode MOE (<0.01–0.05 mm2 vs. 0.75–1.96 mm2). Polarity-reversal experiments revealed a polarity-dependent distribution of iron products, which cannot be explained by thermal reduction alone, suggesting an electrochemical contribution to iron formation. Iron formation observed during plasma MOE is comparable to that of immersed-electrode MOE, although a quantitative evaluation remains challenging. These results provide a proof-of-concept for plasma MOE as an approach that suppresses anode erosion while enabling iron production, indicating its potential as a promising route for carbon-neutral ironmaking.

Steelmaking
Short Article
  • Huafang Yu, Fuga Sato, Takayuki Iwama, Wen-feng Gu, Elizaveta Cheremis ...
    Article type: Short Article
    2026Volume 66Issue 12 Pages 1675-1682
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: October 05, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    To clarify the foaming behavior of FeO-containing slags during pulverized coal injection, calcined anthracite powder was introduced under continuous Ar gas blowing, and the temporal change in foam height was measured. CaO–SiO2–FeO–Al2O3 and CaO–SiO2–FeO–MgO slags were used. Relatively large bubbles were formed when only Ar gas was blown, whereas after pulverized coal injection, a film-like structure formed on the slag surface and the foam height increased markedly. For the Al2O3-containing slag, injection of 0.1 g of pulverized coal resulted in maximum foam heights of approximately 30 mm in the first injection and 65 mm in the second injection. SEM observation and EDS analysis revealed phases corresponding to wüstite, gehlenite, and fine metallic Fe in the upper region of the Al2O3-containing slag, and phases corresponding to wüstite and metallic Fe in the film-like sample from the MgO-containing slag. In foaming caused only by Ar gas blowing, the foam height increased on the higher-viscosity side, whereas during pulverized coal injection, the maximum foam height increased with increasing temperature. The MgO-containing slag showed a lower foam height than the Al2O3-containing slag under Ar gas blowing alone, but exhibited rapid and pronounced foaming during pulverized coal injection. These results suggest that foaming during pulverized coal injection is likely a multiphase reaction phenomenon governed by the combined effects of liquid-phase viscosity, gas generation through the carbonaceous material–FeO reaction, dispersion of solid phases or metallic Fe particles, and gas retention within the foam films.

Forming Processing and Thermomechanical Treatment
Short Article
  • Hajime Kubota, Takuro Masumura, Toshihiro Tsuchiyama, Kento Hani, Misa ...
    Article type: Short Article
    2026Volume 66Issue 12 Pages 1683-1689
    Published: November 15, 2026
    Released on J-STAGE: November 15, 2026
    Advance online publication: September 07, 2026
    JOURNAL OPEN ACCESS FULL-TEXT HTML

    The Fe–10%Mn–0.1%C alloy exhibits an ultra-fine microstructure containing α’-martensite (bcc), ε-martensite (hcp), and retained austenite (fcc). However, Mn causes grain boundary embrittlement and intergranular fracture at prior austenite grain boundaries at low temperatures. In this study, ≦0.9 mass% Mo was added to Fe–10%Mn–0.1%C alloys to suppress intergranular fracture and improve their toughness in their as-quenched states. Electron backscatter and neutron diffraction revealed that Mo addition displayed little influence on the prior austenite grain size, martensitic block width, and phase fractions. Scanning transmission electron microscopy–energy-dispersive X-ray spectroscopy indicated that Mo segregated at the prior austenite grain boundaries at approximately 3 mass% after austenitizing 0.9%Mo steel at 1173 K, whereas Mn segregation remained almost unchanged. Thermodynamic calculations using the Hillert–Ohtani model confirmed that Mo exhibited a stronger segregation tendency than that of Mn. Charpy impact tests indicated that the ductile-to-brittle transition temperature (DBTT) decreased from 275 K for the Mo-free steel to 220 K for the 0.9%Mo steel. Fractographic observations revealed that intergranular fracture, which was dominant in the Mo-free steel at 77 K, was significantly suppressed by Mo addition. In the 0.9%Mo steel, intragranular fracture occurred with a characteristic size corresponding to the block size of α’-martensite. Therefore, Mo segregation effectively strengthens the prior austenite grain boundaries and suppresses intergranular fracture within Fe–10%Mn–0.1%C steel, leading to an improved low-temperature toughness and a reduced DBTT.

feedback
Top