As a countermeasure for restrictions on the use of a large amount of iron ore concentrate in the sintering process, the premixing conditions when using an intensive mixer were studied. First, fine iron ore (−500 μm), which must be agglomerated in the granulation process, was evaluated by adhesion tests, and the effect of premixing on the granule size was evaluated in laboratory and operational plant tests. It was found that the adhesive force of the fine iron ore increased with the decrement of the particle size, and the adhesive force increased greatly with expansion of the size distribution by blending widely different iron ores. As a result of this improvement, the granule size was increased with the intensive mixer when blending fine pellet feed in the raw material at a rate of 15%. As an additional advantage, this improvement could be obtained with a relatively low specific premixing energy. Therefore, it was suggested that this optimization of the blending conditions and premixing is an effective measure for increasing the use of iron ore concentrates.

The effect of Zn content in the α-(Fe, Zn) phase constituting the coating layer on the corrosion resistance of hot-stamped zinc-coated steel sheets was elucidated based on the structural and electrochemical characterization of the corrosion products. Goethite, lepidocrocite, akageneite, and magnetite were the main corrosion products, and the Zn2+ content in the magnetite increased with the Zn content in the α-(Fe, Zn) phase. The increased incorporation of Zn2+ into the magnetite suppressed the cathodic reduction reactions of lepidocrocite and akaganeite, thereby enhancing the corrosion resistance of the steel sheets.

Decarburization slag, a type of steelmaking slag, contains free lime (f-CaO). Slag with a high content of f-CaO tend to disintegrate due to hydration reactions. Since decarburization slag is often pre-hydrated by steam aging for utilization, there is a possibility that it may disintegrate.
In this study, slag prepared by melting was subjected to steam aging treatment, followed by X-ray CT measurements. This process was repeated alternately to evaluate changes in the voids within slag particles.
Slag containing about 2mass% f-CaO showed no increase in voids even after 24 hours of steam aging. On the other hand, slag with f-CaO content of 6mass% or more exhibited an increase in voids after less than 12 hours of steam aging. Especially, slag with an f-CaO content of 9mass% or more showed a marked increase in voids 20 μm in diameter. The growth of fractures was indicated by this increase in voids. Furthermore, it was found that when the void diameter reached 200 to 300 μm, the particles disintegrated.
These results suggest that, in low f-CaO slag, the reaction may be completed at the initial stage of steam aging, whereas in high f-CaO slag, the formation of new fracture surfaces occurs during steam aging. Therefore, slag with high f-CaO content is considered to require a longer steam aging time compared to slag with low f-CaO content. Reducing the proportion of high f-CaO slag is considered to contribute to shortening the time required for steam aging treatment.

The tensile properties and long-term creep strength of KA-SUS321J2HTB were compared with those of KA-SUS304J1HTB, KA-SUS310J1TB, and ASME TP347HFG steels. The 0.2% proof stress and tensile strength of KA-SUS321J2HTB were lower than or equal to those of the other three steels at high temperatures. The tensile ductility of KA-SUS321J2HTB was almost the same as that of the other three steels up to 650°C. The reduction of area in the tensile test decreased at 700 to 800°C for KA-SUS321J2HTB. Creep strength degradation was clearly observed in the long-term for KA-SUS321J2HTB, similar to KA-SUS304J1HTB and KA-SUS310J1TB. However, the creep strength of KA-SUS321J2HTB was higher than those of the other three steels at 650 to 750°C. The same tendency was recognized in the relationship between stress and minimum creep rate. The creep rupture ductility of KA-SUS321J2HTB gradually decreased with increasing time to rupture, as observed for the other three steels.