Abstract
In this study emission from wood-based materials specimen glued with both Epoxy resin adhesives(EP) and Ethylene-Vinylacetate copolymer emulsion adhesives (EVA) contained a slight amount of toluene, xylene, ethylbenzene was measured by using small chamber method according to JIS A 1901. The result of this study,show that it has been understood that the VOC's emission changes due to an internal structure and components characteristic. After 1day the VOC of MDF specimen and PB specimen decreased slightly. Their reason is that the MDF specimen and PB specimen are porous wood-material. Similar VOC's emission behavior was achived by CSB specimen and MDF specimen. VOC's emission behavior of PW specimen decreace gradual.It is suggest that the cause depends on PW adhesion layer.