NIPPON GOMU KYOKAISHI
Print ISSN : 0029-022X
Regular Papers
Scaling of Wear Resistance of Rubber Compounds for Tires Using Rubber Properties
Michio HIRAYAMATakashi NISHINO
Author information
JOURNAL FREE ACCESS

2013 Volume 86 Issue 1 Pages 3-7

Details
Abstract
The tire wear tests were performed for rubber compounds with different physical properties on the different road surface temperature using the same vehicle. It is clear that the temperature dependence of wear resistance were different for the different rubber compounds. The wear resistance W is found to be scaled using the fracture energy F (MJ/m3) and the storage modulus E* (MPa) for the rubber compound as follows:
W = c(Fa / E*b)(a, b, c=the constant number)
Temperature dependence of wear resistance is considered to be caused by the different contribution of F and E* values.
Content from these authors
© 2013 The Society of Rubber Industry, Japan
Next article
feedback
Top