2024 Volume 64 Issue 15 Pages 2144-2148
Towards steelmaking processes which are compatible with the sustainable society, re-sulfurization reaction in hot metal pre-treatments needs to be suppressed as much as possible. To evaluate the effects of iron oxide on the sulfur distribution ratio between FeO-containing slag and hot metal, sulfide capacities and FeO activities were measured in CaO–SiO2–FeO and CaO–Al2O3–FeO ternary liquid slags. Although the FeO activity and oxygen potential increased, the addition of FeO raised sulfide capacity drastically and resulted in an increase in the calculated value for distribution ratio of sulfur.