1992 Volume 100 Issue 1165 Pages 1175-1178
Hydroxyapatite (HAp) powders with SiC platelets dispersion were synthesized by a wet process (at 98°C for 24h) and hydrothermal process (at 150°C, 0.5MPa for 4h). The transmission electron microscopy showed that SiC platelets were homogeneously surrounded by fine HAp crystals. The SiC-HAp composites were sintered at various temperatures. SiC loading obstructed the densification but improved the Vickers hardness up to 1.3 times that of pure HAp ceramics.