Tough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600°C) spark plasma sintering
Petre BADICASalvatore GRASSOHanna BORODIANSKASky Shumao XIEPeifeng LIPeter TATARKOMike J. REECEYoshio SAKKAOleg VASYLKIV
Author information
JOURNAL FREE ACCESS

2014 Volume 122 Issue 1424 Pages 271-275

Details
Abstract

Dense boron carbide (above 95%) was achieved through high pressure (300 MPa) and low temperature (1600°C) Spark Plasma Sintering (SPS). This approach resulted in improvement of fracture toughness and of dynamic toughness when compared to corresponding toughness values of the sample sintered by conventional SPS (2100°C, 50 MPa). Dynamic toughness was extracted from Split Hopkinson Pressure Bar measurements. Results are understood based on microstructure and on very different behaviour of the samples in respect to residual B2O3 and carbon available in the raw B4C powder.

Content from these authors
© 2014 The Ceramic Society of Japan
Previous article Next article
feedback
Top