Journal of the Ceramic Society of Japan
Online ISSN : 1348-6535
Print ISSN : 1882-0743
ISSN-L : 1348-6535
Full papers
Effect of cetyltrimethylammonium bromide to silicon molar ratio on specific surface area of mesoporous silica
Hiroaki Nishiza, Satoshi Tanaka
Author information
JOURNAL OPEN ACCESS

2026 Volume 134 Issue 10 Pages 713-720

Details
Abstract

To synthesize MCM-41 with high-specific-surface-area (SSA) for advanced applications as an adsorbent with designable pore-space architecture, this study focused on the regularity of pore ordering in MCM-41 and the thickness of the silica walls between pores (wall thickness). The effect of the molar ratio of the template molecule cetyltrimethylammonium bromide (CTAB) to tetraethyl orthosilicate (CTAB/Si) on SSA of MCM-41 was systematically investigated. As CTAB/Si ratio increased, SSA of MCM-41 increased and became constant under conditions with CTAB/Si ratios of 0.2 or higher. At CTAB/Si ratio of 0.25, SSA of MCM-41 showed the highest value of 1,688 m2/g. As CTAB/Si ratio increased, wall thickness decreased almost linearly, and SSA of MCM-41 increased. In wall thickness range of 1.4–1.8 nm, SSA of MCM-41 changed linearly, and under conditions with wall thicknesses of 1.4 nm or lower, SSA of MCM-41 showed a constant value of approximately 1,670 m2/g. It was revealed that it becomes possible to control the increase in SSA of MCM-41 by decreasing wall thickness. It was confirmed that an upper limit existed for SSA of MCM-41 obtained under the present experimental conditions. Under conditions at CTAB/Si ratio of 0.15 or higher, where dissolution of amorphous silica in MCM-41 is less likely to occur, it was revealed that a decrease in wall thickness primarily contributes to an increase in SSA of MCM-41.

Content from these authors
© 2026 The Ceramic Society of Japan

この記事はクリエイティブ・コモンズ [表示 4.0 国際]ライセンスの下に提供されています。
https://creativecommons.org/licenses/by/4.0/deed.ja
Previous article Next article
feedback
Top