Article ID: 26073
Tungsten trioxide (WO3) exhibits electrochromic (EC) behavior through reversible ion insertion and extraction. In this study, wet-processed WO3 thin films were fabricated using amorphous-like and crystalline WO3 nanoparticles, and the EC properties of the crystalline WO3 films were evaluated using amorphous-like WO3 as a reference. The effects of aqueous rocking-mill treatment and polyvinyl alcohol (PVA) addition on particle dispersion, film formation, and EC properties were also investigated. The amorphous-like WO3 films showed superior EC performance to untreated crystalline WO3 films. XRD identified the as-received crystalline WO3 as monoclinic and showed that the recovered powder remained crystalline after rocking-mill treatment, with formation of hydrated WO3. Rocking-mill treatment improved particle dispersion and, with optimized slurry conditions, enabled uniform films with clear EC activity, while PVA addition further enhanced optical modulation. These results indicate that the EC performance of wet-processed WO3 films is governed by the combined effects of crystal structure, particle dispersion, slurry rheology, and film formation.