Article ID: 26080
Ultraviolet (UV)-emitting materials have considerable potential for emerging applications, such as photocatalysis and photosterilization. However, the development of such materials is constrained by their requirement for high-energy excitation owing to the Stokes shift. In this study, we focused on optically stimulated luminescence (OSL), which enables the release of stored energy as high-energy emission upon stimulation with long-wavelength light. Based on previously reported energy level diagrams, we synthesized Ce3+–Ln3+ co-doped YPO4 (Ln = Nd, Dy, or Ho) and evaluated its luminescence and OSL properties. Under deep-UV or X-ray irradiation, UV emission from Ce3+ was observed regardless of the co-doped Ln3+ ion. Co-doping with Dy3+ resulted in UV OSL attributed to the Ce3+: 5d–4f transitions under both visible and near-infrared (NIR) stimulation. By contrast, the Nd3+ and Ho3+ co-doped samples exhibited substantially weaker UV OSL because a large fraction of the trapped electrons are thermally released even at room temperature. The OSL stimulation spectrum of YPO4:Ce3+–Dy3+ showed the strongest OSL response under NIR stimulation at approximately 800 nm. An empirical analysis based on the low-spin–high-spin exchange splitting suggests that Dy2+ 4f95d1 excited states may serve as intermediate excited states in the optical detrapping process, although the origin of the main stimulation band remains uncertain. These results demonstrate the potential for tuning OSL stimulation wavelengths through the appropriate selection of co-doped Ln3+ ions and indicate that both trap depths and intermediate excited states must be considered in the rational design of OSL phosphors.