Effects of Sr, Ti-B and Cooling Rate on Solidification Structures of Al-Si-Cu Cast Alloy
Hyogyoung Kang, Hirofumi Miyahara, Keisaku Ogi
Author information
JOURNAL FREE ACCESS

1997 Volume 69 Issue 5 Pages 383-390

Details
Abstract
  The effects of cooling rate and addition of Sr and Ti-B on microstructural features such as grain size, dendrite arm spacing, morphologies of eutectic silicon and iron rich compound were investigated for the Al-6.55%Si-2.78%Cu-0.59% Fe-0.38% Mg-0.34%Mn alloy (JIS AC4B). This alloy solidifies in the order of primary α (Al) , α + α-AlFeMnSi eutectic, α + Si eutectic, α + β-AlFeMnSi eutectic, α + Si + Mg2Si eutectic and α + Si + Al2Cu eutectic. The grain size, dendrite arm spacing, size of eutectic silicon particles and length of needle-like iron rich compound decrease as the cooling rate increases, and they are in linear relation on the logarithmic scale. The addition of a small amount of Ti-B markedly refines the grain size while practically unaffects the other solidification structures. At the cooling rates of 2.7K/s, 14.4K/s and 108.1K/s, the eutectic silicon crystals fully modify with the addition of Sr more than 60ppm, 13ppm and 5ppm respectively. The addition of Sr and a higher cooling rate tends to increase the formation of chinese script type iron rich compound.
Content from these authors
© 1997 Japan Foundry Engineering Society
Next article
feedback
Top