Research Article
Influence of Si and Cooling Rate on Chunky Graphite Formation
Hideo Nakae, Ho-Chul Shin, Manami Hara, Yohei Harada
Author information
JOURNAL FREE ACCESS

2003 Volume 75 Issue 5 Pages 337-343

Details
Abstract
  The formation mechanism of chunky graphite (ChG) was studied using the small droplet method, in which a small iron drop was melted on a pure graphite plate, then cooled at different cooling rates from 1000 K/min to 1.0 K/min in a He-3%H2 atmosphere. We prepared six kinds of samples, namely, pure Fe-C, Fe-C-Si and Fe-C-Ce alloys.
  The graphite morphology of the Fe-C-Ce sample cooled at 20 K/min is mainly spherical and partly chunky. Nevertheless, the carbon morphology of the sample cooled at 40 K/min is mainly spheroidal graphite(SG) and partly ledeburite. The shapes of the ChG area and ledeburite area are identical and look like the residual liquid phase. This means that the residual liquid solidifies to ChG when the cooling rate is less than 20 K/min, but solidifies to ledeburite when the rate is more than 40 K/min.
  The addition of Si to the Fe-C alloy accelerates the formation of ChG. The influence of Ni is identical to that of Si as reported. Si and Ni are graphitizing elements and decrease the graphite volume during eutectic solidification. Therefore, the thickness of the austenite shell surrounding SG becomes thicker with the addition of Si and Ni. The growth of SG during eutectic solidification is controlled by the diffusion of C through the austenite shell. Therefore, the addition of Si accelerates the formation of ChG due to the thickening of the austenite shell. It is thought that ChG forms in the growth SG iron melt due to significant undercooling.