Preparation of Zinc Aluminate Spinel ZnAl2O4 by Corrosion Synthesis in Ethanol
Daichi SASAKIOsami SERI
Author information
JOURNAL OPEN ACCESS

2013 Volume 60 Issue 7 Pages 325-329

Details
Abstract
ZnAl2O4 was obtained by corrosion synthesis which produced mixtures of zinc alkoxide by metallic zinc dissolution in ethanol and aluminum ions by addition of aluminum chloride as a catalyst. The corrosion product became ZnAl2O4 when the mixtures were hydrolyzed, pH-adjusted, and fired at temperature higher than 873 K. It is shown that the ZnAl2O4 powder has the particle size distribution of 0.4 to 10 µm. It is considered that the corrosion synthesis of a ZnAl2O4 production has some features of fast reaction in ethanol and well blending circumstances in ion size level condition.
Content from these authors
© 2013 by Japan Society of Powder and Powder Metallurgy

本論文はCC BY-NC-NDライセンスによって許諾されています.ライセンスの内容を知りたい方は,https://creativecommons.org/licenses/by-nc-nd/4.0/deed.jaでご確認ください.
https://creativecommons.org/licenses/by-nc-nd/4.0/deed.ja
Previous article Next article
feedback
Top