Abstract
Al2O3-dispersed ZrO2-3mol%Y2O3 composites have been prepared by slip casting and electrophoretic deposition to compare the sinterability and microstructure, using three commercially-available Al2O3 powders. Composites were prepared by pressureless sintering at 1300°C. The consolidated (green) density, sintered density, grain size and dispersion are compared for both colloidal techniques with the aim of improving the homogeneity and reducing the necessary temperature for sintering.