The conditions for preparing ThO2-UO3 sol by using the gaseous ammonia addition method are studied. Dependences of colloid particle size and colloid fraction of sol on U content, (Th+U) concentration and ammonia addition mode are observed, and the conditions for preparing sols suitable for gelation in CCI4-ammonia media are found in the range of 1.01.3 mol (Th+U)/l and U content of 030%. Using the resultant sols, the effect of sol concentration on gelation behaviors such as sphericity and cracking is clarified.