1970 Volume 28 Issue 4 Pages 1031-1038
By using a differential type filter the integrated intensity ratios of electron diffraction ring patterns are measured for NaCl, CuCl and BiOCl films. It is observed that these intensities gradually approach kinematical values as the filter potential is increased to values larger than several hundreds electron-volts. This tendency is the same as in the case of Au, Ag and Al films. A method for obtaining the kinematical intensities from the experimental plots is proposed.