1981 Volume 50 Issue 5 Pages 1411-1412
Magnetostriction constants h1 and h2 of Pd–Co alloys containing 5∼60 at% Co have been measured in the temperature range between 77 K and 300 K. The values of h1 and h2 at 0 K determined by the extrapolation increase in magnitude with increasing Co concentration, and reach the maxima of about −3.1×10−4 and −2.9×10−4 at about 15 at% Co, respectively. With further increase of Co, h1 decreases rapidly in magnitude and becomes positive above about 40 at% Co, while h2 decreases gradually without change in sign.