Proceedings of the Asian Pacific Conference on Fracture and Strength and International Conference on Advanced Technology in Experimental Mechanics
Online ISSN : 2433-1279
1.01.203
Conference information
The Width and Height of Striation in Fatigue of 2017-T4 Al Alloy under Two Step Loading condition(Fatigue 1)
Katsuaki FURUKAWA
Author information
CONFERENCE PROCEEDINGS FREE ACCESS

Pages 360-365

Details
Abstract
This paper investigates striation configuration(H/s) under 2-step loading condition. Here, H is striation height and s is striation width. Under condition that vary from low maximum load to high maximum load, no acceleration of crack growth was visible, further H/s remained similar to values found under constant max. load. When load varied from high to low, retardation appeared immediately after varying the load. Striation configuration immediately after varying the load either flat or the H/s value dropped remained to a level much smaller than that under constant max. load. Once crack growth reached about 500μm, striation configuration recovered from the previous flat condition and the H/s value returned to the value found under constant max. load.
Content from these authors
© 2001 The Japan Society of Mechanical Engineers
Previous article Next article
feedback
Top