2025 Volume 71 Issue 4 Pages 54-61
We investigated the effects of blending polycarbonate (PC) into polypropylene (PP) on the thermal shrinkage and bonding properties of melt-blown nonwoven separators. Each sample was produced by melt-blowing, and the throughput rate and sampling speed were set according to the calculated PC basis weight of 0.7–7 g/m2. The dimensional changes by heating and the changes in the surface state during heating were quantitatively analyzed. Consequently, there was no impairment of the battery characteristics when the PC basis weight was 1.0–4.0 g/m2. The number of thick fibers in the nonwoven increased as the PC basis weight increased. Similarly, the distribution of pore size expanded, but the distribution did not change by heating at 100–140 °C. Thermal shrinkage decreased significantly with increasing PC basis weight in the range 100–120 °C, whereas the tendency reversed above 140 °C. The melting behavior at 160 °C was observed by fixed-end heat treatment; the PP single-component nonwoven melted, but the nonwoven containing PC maintained its morphology. The PP melt gathered around the PC fibers, resulting to form PP membrane in some areas. This suggests that mixed nonwovens have potential shutdown functions.