Abstract
On the friction stir welding (FSW), pre-heating makes welding speed higher, as it makes weld materials more softened. In this study, FSW was done, pre-heated at 150 to 250 degrees Celsius. As the result, the welding speed up to 2000mm/min was got at 250 degrees Celsius.