1985 Volume 1985 Issue 12 Pages 2342-2344
Preparation of spherical silver particles was examined by using spray-pyrolysis technique from AgNO3 solution. The solvent was a mixture of H2O and C2H5OH (25-100 vol%). Although Ag particles were produced by pyrolysis above 650°C, the particles became solid and spheikir when the pyrolysis was done at temperatures higher than melting point of silver. The particle sizes were determined mainly by the degree of the splitting of atomized droplets during the heating process.