Abstract
In this study, the improvement in compressive strength of matrix part in the system of calcium silicate hydrate was aimed by the reduction of the water powder ratio. Further, the morphology and reaction mechanism of autoclaved calcium silicate hydrates in low water powder ratio were studied.