Abstract
Preparation of ZrSiO4/LaPO4 composites and its mechanical properties were studied. ZrSiO4 powder was mixed with highly sinterable LaPO4 powder by a wet precipitation method. The powder was pressed and sintered at 1550°C for 3hr. The XRD pattern of body sintered showed that two phases didn't react and decomposite. The relative density of ZrSiO4/LaPO4 composites was around 96 %. The more we added LaPO4 to ZrSiO4, the more fast drilling rate was. Thus we succeeded to prepare machinable ZrSiO4/LaPO4 composites.