Abstract
The electrical conductivity of lithium borohydride (LiBH4) measured by the ac complex impedance method increased by three orders of magnitude due to structural transition from orthorhombic to hexagonal at approximately 390 K. Spin-lattice relaxation time (T1) of 7Li nuclear magnetic resonance (NMR) was in good agreement with the measured electrical conductivity.