THERMAL BEHAVIOR OF LEAD CYCLO-TRIPHOSPHATE
HIROYUKI NARIAITETSUYA TATSUKAWAHIDESHI MAKIITARU MOTOOKA
Author information
JOURNAL FREE ACCESS

1998 Volume 8 Pages 113-118

Details
Abstract

Lead cyclo-triphosphate (P3m) was synthesized and its thermal behavior was investigated by DTA-TG, XRD, and HPLC-FIA. It hydrolyzed to various short-chain lead phosphates at about 200°C, and they condensed to long-chain lead polyphosphate through lead cyclo-tetraphosphate (P4m) and cyclo-octaphosphate (P8m), or directly condensed to long-chain lead polyphosphate.
For the purpose of increasing the yield of P8m, the thermal change of P3m at various heating rates was investigated. P8m was obtained in a 90% yield at heating rate of 3°C/min, while its yield at 20°C/min was about 30%.