1956 Volume 25 Issue 9 Pages 506-511
Phosphor deoxidized copper and also tough pitch copper plates of 3-4mm thickness were butt welded with nitrogen-arc welding process. Welding conditions such as nitrogen flow, welding current, arc length and travelling speed were selected properly, Good weld result was obtained only when silicon deoxidized copper was used as a filler rod.