Fluidization and Degradation Characteristics of Iron Ore Fines in Prereduction Fluidized Bed
Tatsuro ARIYAMAShinichi ISOZAKIShinji MATSUBARAHitoshi KAWATAIsao KOBAYASHI
Author information
JOURNAL OPEN ACCESS

1993 Volume 79 Issue 12 Pages 1317-1322

Details
Abstract
The integrated test plant, consisting of a prereduction fluidized bed and in-bath smelting furnace characterized by high post combustion, was installed at NKK's Fukuyama Works, and the operation was started in 1988. The prereduction fluidized bed uses iron ore fines as feed, and the fluidizing condition and pressure fluctuation characteristics to keep the stable fluidizing were clarified by the operation of the integrated test plant. The classification behavior of fines was analyzed by the measurement of the elutriation rate constant. Then, the degradation phenomena of iron ore fines were observed during the preheating and prereduction of iron ore fines in the fluidized bed, and it was quantitatively analyzed by the application of Rittinger's law for size reduction. The model including classification and degradation behavior was constructed so as to estimate the operating condition. These results were considered to be availabe in the scale-up of the prereduction fluidized bed.
Content from these authors
© The Iron and Steel Institute of Japan

This article is licensed under a Creative Commons [Attribution-NonCommercial-NoDerivatives 4.0 International] license.
https://creativecommons.org/licenses/by-nc-nd/4.0/