Abstract
This study discusses the heat teat treatment temperature on functional degradation properties. Tensile tests and cyclic tensile loading-unloading tests have been carried out using Ti-50.3at%Ni wires heat-treated at 673K, 723K and 773K for 3.6ks. The tensile strength and the breaking strength decrease increasing heat treatment temperature. The number of cycles to failure increases with increasing heat treatment temperature. However, the effect of maximum applied strain on the number of cycles to failure is small. The cumulative residual strain increases with increasing heat treatment temperature and it increases with increasing number of cycles. In addition, the cumulative residual strain of heat treatment temperature of 773K rapidly increases with increasing number of cycles during the first 10 cycles. The stress for inducing martensite decreases with increasing heat treatment temperature and it decreases with increasing number of cycles. The maximum stress decreases with increasing heat treatment temperature. The maximum stress of the maximum applied strain of 10% rapidly decreases with increasing number of cycles during the first 10 cycles.