Four kinds of carbon composite iron ore briquette (CCB) were made by mixing two kinds of iron ores and coals that have different properties such as hematite, magnetite, fluidity and non-fluidity coal. The reaction behavior of those CCB was examined at the temperatures of 1273–1473K in N2 gas atmosphere. The effect of iron ore and coal properties on reaction behavior of CCB was investigated. In the case of CCB that mixed fluidity coal, gasification and reduction rates of the CCB were fast because the contact of iron ore and coal improved. In the case of CCB that mixed hematite ore, reduction rate of the CCB was fast because the reduction rate of hematite ore is faster than that of magnetite ore. Therefore, the reaction rate of CCB that mixed fluidity coal and hematite ore was the fastest in samples.

著者関連情報
© 2009 一般社団法人 日本鉄鋼協会

This article is licensed under a Creative Commons [Attribution-NonCommercial-NoDerivatives 4.0 International] license.
https://creativecommons.org/licenses/by-nc-nd/4.0/
次の記事
feedback
Top