延伸倍率の連続変化に対する繊維直径の応答性
的場 兵和伊藤 章喜伊香賀 敏文大越 豊
著者情報
ジャーナル フリー

2014 年 70 巻 8 号 p. 167-173

詳細
抄録
The fiber with gradually changing diameter was fabricated by changing the draw ratio continuously, that is, by changing the take-up speed of melt spinning, laser drawing, and heater drawing processes. The diameter profiles of resultant fibers were monitored and compared each other. As the results, the laser drawing shows the best diameter responsiveness among the three. For the case, the diameter changing rate increased with the increase of fiber acceleration rate up to 6.0 m/s2. Moreover, it can make the fiber whose diameter gradually changed about 40% within 8 cm range for the minimum case. The diameter profile was determinded by not only the draw ratio profile but also the start/end draw ratios. The lower drawing stress change tends to improve the responsiveness, and the minimum response length for laser drawing was obtained for the draw ratio decreasing case.
著者関連情報
© 2014 The Society of Fiber Science and Technology, Japan
前の記事 次の記事
feedback
Top