International Chinese Journal of Dentistry
Online ISSN : 2759-9108
Print ISSN : 1608-0688
Original Article
The effect of the dentin preparation with an ultrasonic abrasion on the microtensile bond strength of self-etch adhesive systems
Hiroyuki Takanashi , Keiichi Hosaka, Ryuzo Kishikawa, Masayuki Otsuki, Junji Tagami
Author information
JOURNAL FREE ACCESS

2010 Volume 10 Issue 1 Pages 7-15

Details
Abstract

Purpose: This study evaluated the effect of the dentin preparation with an ultrasonic abrasion on the microtensile bond strengths (µTBS) of two-step and one-step self-etch adhesive systems to dentin.
Materials and Methods: A two-step self-etch adhesive, Clearfil SE Bond (Kuraray Medical) and a one-step self-etch adhesive, Clearfil S3 Bond (Kuraray Medical) were applied on dentin prepared with a diamond-coated round working tip, Excavus (EX, Satelec) activated through ultrasonic frequency oscillations, with a regular grit diamond bur (DB) in a turbine handpiece, with a steel bur (SB) in a micromotor handpiece, or with a #600 grid silicon carbide abrasive paper (SiC). Then, a photo-cured composite was placed and polymerized. The µTBS was measured after storage in water for 24 hours at 37˚C. The data were statistically analyzed using a two-way ANOVA and Dunnett’s C test at 95% level of confidence. The prepared surfaces and their crosscut surfaces were observed using a scanning electron microscope (SEM).
Results: For Clearfil SE Bond, the µTBS of EX was higher than that of DB and there were no differences among EX, SB, and SiC groups. For Clearfil S3 Bond, the µTBSs of EX and DB were lower than those of SB and SiC. The µTBS values of Clearfil SE Bond were significantly higher than Clearfil S3 Bond, irrespective of the dentin preparation methods. The two-way ANOVA analysis revealed that there was a significant interaction between the dentin preparation methods and the adhesive systems (p<0.05). Bond strength was influenced by the dentin preparation method (p<0.05) and by the adhesive systems (p<0.05). SEM observation of the dentin surfaces prepared with EX showed the thicker and uneven smear layers, compared with SB and SiC.
Conclusion: The µTBS to dentin prepared using an ultrasonic abrasion with EX, when Clearfil SE Bond was applied, was similar to SB and SiC groups and higher than DB group. However, when Clearfil S3 Bond was applied, the µTBS to dentin prepared with EX was statistically lower than SB and SiC groups and were similar to DB group. The mean µTBSs of Clearfil SE Bond were higher than those of Clearfil S3 when using the same dentin surface preparation.

Content from these authors
© Japanese Dental Science Federation
Previous article Next article
feedback
Top