Abstract
According to Chvorinov, solidification time of a sand casting is determined by the ratio of the volume of the casting to its surface area:
tf=K(V/S)2
where K is considered a constant independent of the shape of the casting. The dependence of K on the shape of casting was discussed theoretically by examining the interface temperature between casting and mold. Plate, cylinder and sphere were chosen as the typical shapes. Pure metal and zero superheat were assumed. The following conclusions were obtained.
(1) The interface temperature during solidification depends on the thermal properties of the cast metal, the mold material and the shape of casting (eq. (17)). It is independent of the size of casting.
(2) In addition to the Adams' correction with respect to the contour effect, interface temperature correction must be made for Chvorinov's rule (eq. (19)).
(3) After the two corrections, it was shown that the dependence of K on shape is governed by the factor B/L, where B=b1/b2 is the relative heat diffusivity (suffix 1 for mold and 2 for metal) and L=L2/c2θf is the relative latent heat of solidification. For small B/L (<0.1) K for cylinder and sphere are smaller than K for plate (e. g. Al or Cu cast in sand mold). For large B/L (>0.3) K for cylinder and sphere are larger than K for plate (e. g. steel cast in high diffusivity sand). Only when B/L is of intermediate value (0.1-0.3), K is independent of casting shape and Chvorinov's rule is satisfied with high precision (e. g. steel cast in low diffusivity sand).