抄録
Commercial heats of Cr and Cr-Mo bearing dual phase steels have been hot rolled by keeping roll finish temperature in the range of 850-880°C and varying the coiling temperature between 200 and 570°C. Mechanical test and retained austenite measurement have been carried out on samples collected from different locations of coils (representing different cooling rates between Ms and Mf temperatures) and also on some of the as received samples which have been given selective heat treatment. The reason for wide range of retained austenite (varying between 0-16%) has been given based on the stability criteria of austenite. Effect of retained austenite on mechanical properties has been discussed and a distinct beneficial effect of retained austenite on mechanical properties, particularly elongation has been found.