Size Degradation of Deadman Coke by Reaction with Molten FeO in Blast Furnace
Kohei SunaharaTakanobu InadaYuji Iwanaga
著者情報
ジャーナル フリー

1993 年 33 巻 2 号 p. 275-283

詳細
抄録

Since particle size of deadman coke greatly affects the permeability of gas and liquid in the lower part of a blast turnace, elucidation of the behavior of the replacement of deadman coke is an important subject. This paper describes the degradation of deadman coke by t he reaction with molten FeO. With use of a one-dimensional reaction model in which two kinetic parameters were determined from a fundamental experiment, the degradation of the deadman coke in an actual blast furnace was simulated. The effect of FeO in molten slag on the degradation of deadman coke concerns reduction ratio on the melting down of ore, temperature, and productivity. It takes about 2 weeks that vertical size distribution of degrading deadman coke becomes stationary pattern.

著者関連情報
© The Iron and Steel Institute of Japan
前の記事 次の記事
feedback
Top