Oxidation of Carbon Monoxide with Air on Supported Palladium Catalysts: Effect of Mass Transfer Limitation on the Kinetics
Françoise DupratHector Romo Moreno
著者情報
ジャーナル 認証あり

2000 年 33 巻 3 号 p. 400-406

詳細
抄録
The kinetics of oxidation of carbon monoxide on Pd-supported catalysts are determined at low temperature and under typical conditions of atmospheric pollution (a few ppm of CO in air). The nature (silica, alumina, silica-alumina) as well as the geometry (beads, fibers, powder) of the support were varied, the latter to change the mass-transfer resistance. The nature of the support has no influence on the kinetics. With powder or fiber as the supports, the catalyst operates without mass transfer limitation, and the kinetics is of negative order with respect to CO, of positive order with respect to oxygen. The energy of activation is about 85 kJ/mol. This corresponds to the regime of CO-inhibition, never reported at so high O2 to CO ratio (75–104). The surface is dominated by adsorbed carbon monoxide, and the reaction rate is limited by oxygen adsorption. With beads as the support, the orders in CO and in oxygen are both positive and the energy of activation is 42 kJ/mol. This kinetics law is attributed to mass transfer limitation.
著者関連情報
© 2000 The Society of Chemical Engineers, Japan
前の記事 次の記事
feedback
Top