1978 Volume 42 Issue 6 Pages 606-611
Tension and tensile fatigue tests of water-quenched Cu-Al alloy (β2 phase) with 10 wt%Al have been performed at high temperature in vacuum. The relations among tensile strength σB (strain rate 0.003 s−1), temperature T, cyclic tensile stress (of maximum value σ0) and fatigue life N (number of stress cycles to fracture) are approximately given by
(This article is not displayable. Please see full text pdf.)
\
oindentwhere N0=103, B=10, σB*=8.24×108 Pa, B*=−6.5×10−6 K−2, and T0=270 K.
The expression of the tensile fatigue strength derived from known condition of fatigue failure and deformation is found to agree with the above experimental relation.