Effect of Homogeneity in Sintered Material’s Microstructure on Fatigue Strength
Fumihiro MaezawaTakayuki TashiroShigeki EgashiraKazunari ShimauchiTomoyuki Ishimine
著者情報
ジャーナル オープンアクセス

2025 年 72 巻 Supplement 号 p. S41-S46

詳細
抄録

Sintered parts can be mass-produced with high precision and cost-effectiveness, and have a wide range of applications, including in automobiles. Since conventional sintered materials tend to show lower fatigue strength than that of wrought steel, they cannot be applied to high load applications.The effect of homogeneity in the microstructure of sintered materials on fatigue strength has been investigated in many studies. In this paper, we compare fatigue strength between homogeneous and heterogeneous materials. Our study reveals that in a high-density range of about 7.7 g/cm3, cracks occur at the surface starting point, and homogeneous materials have a fatigue life 10 times longer than that of heterogeneous materials.

著者関連情報
© 2025 by Japan Society of Powder and Powder Metallurgy

本論文はCC BY-NC-NDライセンスによって許諾されています.ライセンスの内容を知りたい方は,https://creativecommons.org/licenses/by-nc-nd/4.0/deed.jaでご確認ください.
https://creativecommons.org/licenses/by-nc-nd/4.0/deed.ja
前の記事 次の記事
feedback
Top