射出成形体の抽出脱脂
笠原 範雄斎藤 勝義寒川 喜光金子 泰成
著者情報
ジャーナル オープンアクセス

1991 年 38 巻 6 号 p. 774-776

詳細
抄録
When Producing P/M parts by the MIM, the debinding step takes the longest time of its process. How to reduce the binder removal time is the key to the MIM, though the injection machine forming is highly productive. The rapid binder removal could be achived by the solvent extraction. When using copper powder, the solvent extraction needed 8 houus, though the thermal debinding needed more than 40 hours. The sintered pert at 1020°C had a relative density of 95%. The pore was all closed, which was remarkable of the MIM sintered part. Two types of the binder were discussed here. One consisted of polyolefin and oil, another consisted of polyethylene glycol. Using the polyethylene glycol, the miscibility of the binder had been much improved.
著者関連情報
© 社団法人粉体粉末冶金協会

本論文はCC BY-NC-NDライセンスによって許諾されています.ライセンスの内容を知りたい方は,https://creativecommons.org/licenses/by-nc-nd/4.0/deed.jaでご確認ください.
https://creativecommons.org/licenses/by-nc-nd/4.0/deed.ja
前の記事 次の記事
feedback
Top